Shortcomings in
Causes
Solution
orange peel
① paint too high viscosity, or a spray too much.
② volatile solvent too fast, resulting in flow-coating bad.
③ improper spraying distance, not enough pressure air compressor, paint atomizing bad.
④ coatings and solvents have absorbed moisture.
⑤ leveling paint their own poor.
⑥ coating before sanding adverse impact of the leveling of paint.
⑦ bottom paint is not fully dry.

① adjustment of viscosity, choose the right calibre of Lance, one-time reduction of spraying.
② season under climate change, choose the appropriate thinner.
③ adjustment pressure air compressor, spraying a good distance control.
④ remaining paint and solvent kept sealed when attention.
⑤ before the full use of mixing paints, coatings enhance the leveling.
⑥ sanding to smooth.
⑦ repeatedly spraying, to ensure that the full bottom paint dry.
 
     
     
   
 